Home to one of the world’s most comprehensive nanocellulose manufacturing platforms, Cellulose Lab provides industrial-scale CNF, CNC, and BC solutions engineered for performance, consistency, and commercial success.

Advanced Nanocellulose Materials for Industrial Scale

At Cellulose Lab, we deliver engineered nanocellulose solutions designed for demanding industrial applications. Combining scientific expertise, manufacturing excellence, and scalable production capability, we support global customers in accelerating innovation across coatings, composites, specialty chemicals, energy materials, life sciences, packaging, and advanced manufacturing.

Our portfolio includes Cellulose Nanofibers (CNF)Cellulose Nanocrystals (CNC), and Bacterial Cellulose (BC), supported by one of the industry’s most comprehensive nanocellulose platforms. From standard production grades to highly engineered functional materials, our products are designed to deliver consistent performance, process reliability, and seamless integration into commercial manufacturing environments.

Built on deep expertise in cellulose chemistry, surface engineering, colloidal science, and process optimization, we offer extensive customization capabilities—including fiber morphology, surface functionality, charge density, counter-ion selection, solids content, viscosity control, and application-specific performance tuning. Whether supporting early-stage formulation development or full-scale commercialization, our technical team works as an extension of your R&D and manufacturing organization.

Quality, consistency, and supply reliability are at the core of everything we do. Every production lot is manufactured under rigorous process control and validated through comprehensive analytical characterization to ensure batch-to-batch consistency at industrial scale.

For industrial partners, we offer highly competitive commercial pricing, with additional strategic pricing programs available for routine procurement, long-term supply agreements, and high-volume manufacturing. Combined with responsive technical support, flexible production scheduling, and global logistics capability, Cellulose Lab is committed to being your trusted long-term materials partner.

Industrial Product Portfolio

A comprehensive portfolio of engineered CNF, CNC, and BC materials, available in multiple fiber architectures, surface chemistries, functional modifications, and commercial production grades—designed to meet the performance requirements of modern industrial systems.

CNF Product CatalogueProduct DescriptionMOQ (kg, dry basis)Price (USD $/kg, dry basis)
MFC-Slurry-M120Width: 0.2-20 um;
Length: 100-1000 um;
D50: 125 um;
100 um (%): > 30%;
SSA: 0.045 m²/g;
Surface Group: Hydroxyl;
Hydrophilic
2.5 tons dry weight
Maximum Solid Content: 20%
33
MFC-Slurry-M100Width: 0.05-20 um;
Length: 20-200 um;
D50: 93 um;
100 um (%): > 40%;
SSA: 0.056 m²/g;
Surface Group: Hydroxyl;
Hydrophilic
2.5 tons dry weight
Maximum Solid Content: 20%
33
MFC-Slurry-M70Width: 0.01-1 um;
Length: 1-100 um;
D50: 69 um;
100 um (%): > 50%;
SSA: 0.076 m²/g;
Surface Group: Hydroxyl;
Hydrophilic
2.5 tons dry weight
Maximum Solid Content: 20%
35
CNF-Slurry-H50Width: 1-80 nm;
Length: 1-50 um;
D50: 50 um;
100 um (%): > 70%;
SSA: 0.077 m²/g;
Surface Group: Hydroxyl;
Hydrophilic
1 tons dry weight
Maximum Solid Content: 15%
40
CNF-Slurry-H35Width: 1-50 nm;
Length: 1-30 um;
D50: 35 um;
100 um (%): > 85%;
SSA: 0.084 m²/g;
Surface Group: Hydroxyl;
Hydrophilic
1 tons dry weight
Maximum Solid Content: 15%
43
CNF-Slurry-H25Width: 1-30 nm;
Length: 1-10 um;
D50: 24 um;
100 um (%): > 95%;
SSA: 0.14 m²/g;
Surface Group: Hydroxyl;
Hydrophilic
1 tons dry weight
Maximum Solid Content: 15%
45
CNF-Slurry-B20Width: 5-30 nm;
Length: 50-300 nm;
D50: 21.5 um;
100 um (%): > 95%;
SSA: 0.24 m²/g;
Viscosity: 174 – 210 mPa.s;
Surface Group: Hydroxyl;
Hydrophilic
1.5 tons dry weight
Maximum Solid Content: 10%
35
CNF-Slurry-B15Width: 5-30 nm;
Length: 50-300 nm;
D50: 18.6 um;
100 um (%): > 98%;
SSA: 0.26 m²/g;
Viscosity: 523 – 568 mPa.s;
Surface Group: Hydroxyl;
Hydrophilic
1.5 tons dry weight
Maximum Solid Content: 10%
35
CNF-Slurry-B10Width: 5-30 nm;
Length: 50-300 nm;
D50: 12 um;
100 um (%): > 99%;
SSA: 0.3 m²/g;
Viscosity: 2860 – 3320 mPa.s;
Surface Group: Hydroxyl;
Hydrophilic
1.5 tons dry weight
Maximum Solid Content: 10%
35
CNF-Slurry-B5Width: 5-30 nm;
Length: 50-300 nm;
D50: 9.3 um;
100 um (%): > 99%;
SSA: 0.4 m²/g;
Viscosity: 15510 – 16940 mPa.s;
Surface Group: Hydroxyl;
Hydrophilic
1.5 tons dry weight
Maximum Solid Content: 10%
35
CNF-Anionic-1.9-STEMPO modified CNF
High charge density (~1.9 mmol/g)
Short fiber length
1 tons dry weight
Maximum Solid Content: 2%
150
CNF-Anionic-1.2-LTEMPO modified CNF
Medium charge density (~1.2 mmol/g)
Long fiber length
1 tons dry weight
Maximum Solid Content: 2%
120
CNF-Anionic-0.5-XLTEMPO modified CNF
Low charge density (~0.5 mmol/g)
Extra long fiber length
1 tons dry weight
Maximum Solid Content: 2%
120
CNF-Cationic-0.6-LCationic type CNF
Medium charge density: ~0.6 mmol/g charge
Long fiber length
0.5 tons dry weight
Maximum Solid Content: 1%
300
CNF-Cationic-1.0-SCationic type CNF
High charge density: ~1.0 mmol/g charge
Short fiber length
0.5 tons dry weight
Maximum Solid Content: 1%
300
CNF-Cationic-0.5-XLCationic type CNF
Low charge density: ~0.5 mmol/g charge
Extra long fiber length
0.5 tons dry weight
Maximum Solid Content: 1%
300
CNF-SBCLower-cost substitute for bacterial cellulose
Surface charge density:0.5mmol/g
0.5 tons dry weight
Maximum Solid Content: 1%
100
CNC Product CatalogProduct descriptionMOQ (kg, dry basis)Price (USD $/kg, dry basis)
CNC-COM-SACellulose Nanocrystals slurry prepared by sulfuric acid hydrolysis
Surface Group: Hydroxyl, sulfonic group, Hydrophilic
100 kg dry weight
Maximum Solid Content: 10%
55 
CNC-COM-TEMPOCellulose Nanocrystals slurry prepared by TEMPO oxidation
Surface group:Hydroxyl, Carboxylated group
Surface charge density:  3 levels, ranging from 0.3 to 2.0 mmol/g
Salt form: sodium (-COONa), lithium (-COOLi), or carboxyl (-COOH)
100 kg dry weight
Maximum Solid Content: 10%
50 
CNC-COM-CationicCationic type Cellulose Nanocrystals slurry125 kg dry weight
Maximum Solid Content: 8%
50 
CNC-COM-ZWZwitterionic Cellulose Nanocrystals slurry
Surface group:Hydroxyl, Quaternary ammonium
Surface charge density:1.0 ± 0.2 mmol/g
Surface group:Hydroxyl, Quaternary ammonium, Carboxylated group
Surface charge density:
Carboxylate group 1.0 ± 0.2 mmol/g
Quaternary ammonium 0.4 ± 0.15mmol/g
100 kg dry weight
Maximum Solid Content: 11%
80 
CNC-COM-HClHydrochloric Acid-Hydrolyzed Cellulose Nanocrystals slurry
Surface group:Hydroxyl
Surface charge density: 0 ± 0.01mmol/g
100 kg dry weight
Maximum Solid Content: 15%
50 
CNC-COM-AEAcetylated (Acetate-Esterified) Cellulose Nanocrystals Slurry100 kg dry weight
Maximum Solid Content: 15%
65 

For BC commercial bulk orders, please contact us at contact@celluloselab.com